The stone itself was structurally sound — limestone tends to fail by surface degradation, not structural collapse. But the visual character was steadily eroding, and without intervention, more of the carved detail would be lost.
The Work
This was an LPC-coordinated project. The application phase took several weeks before any on-site work; we documented existing conditions, specified materials, and submitted for staff approval. Once approved, we proceeded with: gentle cleaning (no harsh acid washes — they would have destroyed the surface), consolidation treatment to strengthen weakened areas, color-matched limestone patching at the most damaged sections, and a final mineral-based painted finish that LPC had approved.
The result
The carved detail is preserved and stabilized. The stone is no longer actively losing material. The painted finish protects the surface for the next maintenance cycle without trapping moisture (mineral-based paint is vapor-permeable, unlike many off-the-shelf options).